[email protected]

Cavitation Erosion and Corrosion Behavior of NiTi Cladding

Jun 22, 2020 · The ranking according to the cavitation erosion resistance is NiTi plate > NiTi-Cu-TIG cladding NiTi-Cu-Nb-TIG cladding > stainless steel. The superior cavitation erosion resistance of NiTi-Cu-TIG and NiTi-Cu-Nb-TIG claddings results from high hardness, superelasticity, no cracks and no brittle Fe 2 Ti phases. However, the corrosion resistance of NiTi claddings with Cu and Cu + Nb Cavitation erosion and corrosion behaviors of laser Tests were conducted for pure cavitation erosion in distilled water, pure corrosion using in-situ electrochemistry under 3.5% NaCl solution, and a combination of cavitation erosion-corrosion to

Cavitation erosion behavior and surface morphology

Cavitation erosion behavior and surface morphology evolution of 316LN austenitic stainless steel in 3.5% NaCl Solution Zhisong Shao 1, Shuaixing Wang,*, However, in addition to pitting, intergranular corrosion and SCC, the 316LN SS elbow used in the AP1000 nuclear power plant may also suffer from cavitation erosion at the bends and stenosis Effect of Passive Film on Cavitation Corrosion Behavior of cavitation erosioncorrosion behavior of the materials, produced an intermittent pressure field, thus inducing the periodic growth and collapse of the cavitation bubbles. Thus, the current study carried out the pulsed cavitation erosion tests by employing 3secon/3 Effect of Sulfide Concentration on the Corrosion and Jun 26, 2019 · The cavitation erosioncorrosion synergy was lower in high sulfide solutions, because the corrosion products on MAB could reduce the mechanical impact under cavitation erosion. The effect of sulfide concentration on the corrosion and cavitation erosion behavior of a cast manganese-aluminum bronze (MAB) alloy in 3.5% NaCl solution

(PDF) Study on Cavitation ErosionCorrosion Behavior of

The sample self-vibration in a cavitation environment was firstly measured and its erosioncorrosion behaviors at ultrasonic generator output powers of 40, 70, and 100 W were fully investigated.